آجر های شاموتی
آمار بازدید:
13916
|
|
|
| |
|
Fireclay Brick AZAR – A40A
|
AZAR - A40A
Chemical Analysis
AL2O3
| %
| Min 40
| Fe2O3
| %
| Max 2
| SiO2
| %
| Max 55
|
Physical Properties
Bulk Density (Db.)
| g/cm3
| 2.10-2.30
| Apparent Porosity (Po.)
| Vol-%
| 10-16
| Cold Crushing Strength (c.c.s)
| kg/cm2
| 350-600
| Thermal Shock Resistance (TSR-H2O)
| cycles
| 15
| Refractoriness Under Load (differential)
| T0.5ºc
| Min 1330
| Refractoriness | ºC
| 1730
|
|
|
|
|
|
Fireclay Brick AZAR – A40B
|
AZAR - A40B
Chemical Analysis
AL2O3
| %
| Min 40
| Fe2O3
| %
| Max 2.80
| SiO2
| %
| Max 55
|
Physical Properties
Bulk Density (Db.)
| g/cm3
| 2.10-2.30
| Apparent Porosity (Po.)
| Vol-%
| 10-16
| Cold Crushing Strength (c.c.s)
| kg/cm2
| 350-600
| Thermal Shock Resistance (TSR-H2O)
| cycles
| 15
| Refractoriness Under Load (differential)
| T0.5ºc
| Min 1320
| Refractoriness | ºC
| 1700
|
|
|
|
|